How to use our metal extraction reagent to process the metals of below?
Ni | Co | Mn | Zn | Ca | Fe | Al | Si | Cu | Mg | |
---|---|---|---|---|---|---|---|---|---|---|
Processed ore | 38 | 2.9 | 4.82 | 1 | 0.15 | 0.36 | 0.36 | 0.19 | 0.12 | 2.3 |
Waste battery liquid 1 | 6.64 | 15.6 | 4.86 | 20.3 | 14.36 | |||||
Waste battery liquid 2 | 10.91 | 14.99 | 10.32 | 0.97 | 9.82 | 1.68 |
1. Use P204 to remove the impurities.
2. Saponify the liquid to 45%, keep temperature to around 50°C.
3. For first one use 15%-20% DZ272, in valume ratio of 1:1 Organic phase to Aqueous phase;
For second one, use 15%-20% DZ272, in valume ratio of 2:1 Organic phase to Aqueous phase;
For third one, use 20% DZ272, in valume ratio of 2:1 or 3:1 Organic phase to Aqueous phase;
Extraction process in 3 to 5 steps.