DY973N extract de cupru is used for the copper selective recovery in the hydrometallurgical processing of copper ores. It is a high-performance hydroxyoxime compound solvent extraction (S X) reagent for copper ions. Specifically used for SX-EW circuits that treating high-content copper ores and low-pH heap leaching solutions.
This image shows the results of our copper extraction experiment, providing a clear understanding of its extraction principle:

This is the actual copper extraction plant, you can see the extracted pure copper sulfate:

Following are the instructions of DY973N:
1. Compoziție chimică & Blending Ratio of DY973N:
Active Ingredients: 5-nonyl salicylaldoxime (Aldoxima) combined mixed with 2-hydroxy-5-nonyl acetophenone oxime (Ketoxima).
Typical Active Ratio: Formulated in an optimized 7:3 volume ratio of aldoxime to ketoxime, includes 35% aldoximă, 15% ketoxima si 50% 260# ulei solvent. The high aldoxime percentage delivers severe copper-loading payloads, while the paired ketoxime functions as a mild kinetic modifier.
2. Performance Parameters of DY973N:
| Physical form: | Technical Value |
| Aspect | Fluid amber oil liquid |
| Densitate (25°C) | 0.91-0.93 |
| Punct de aprindere | ≥62°C (PMCC) |
| Copper complex solubility (25°C) | ≥30 g/L Cu |
| Performance specifications: | |
| Maximum copper loading 10% (V/V) | 5.4-5.7 g/L Cu |
| Punct izoterm de extracție (Organic) | ≥4.7 g/L Cu |
| Cinetica extractiei | ≥95% (30s) |
| Extraction Cu/Fe selectivity | ≥2300 |
| Extraction phase separating | ≤70 de ani |
| Strip isotherm point | ≤2.0 g/L Cu |
| Net copper transfer | 2.7 g/L Cu |
| Strip kinetics | ≥95% (30s) |
| Strip Phase separating | ≤80 de ani |
3. The Advantages of DY973N copper extractant:
Reduced Reagent Consumption: In practica, the consumption of single aldoxime will be 10 kg per metric ton cathode copper, but the consumption of DY973N will be under 5 kg per metric ton, will save the operating cost. Asa de, you can top up the active organic phase with DY973N copper extractant in any ratio.
Superior Iron Rejection: With a selectivity threshold surpassing 2,300, will effectively lock out ferric iron.
4. Application scopes of DY973N copper extractant:
High-Grade Copper Leaching: Used for circuits encountering highly concentrated base metal PLS.
Low-pH Heap & Leşierea: Ideal for mineral acid levels in the pregnant leach solution (PLS) fluctuate significantly or sit at low baselines.
Recycle Scrap Processing: To recycle copper from industrial etching effluents.
Therefore, if you want to verify the miscible compatibility of DY973N with your current active organic phase, va rog sa ne contactati.
Apropo, extractanții noștri de metal, ca mai jos, dacă ai nevoie, nu ezitați să ne întrebați:
- P204 (D2EHPA or HDEHP) This is used for first step to remove impurity for laterite nickel ore.
- P507 non-ferrous metal extractant for copper, zinc, cobalt-nickel, cadmium, gold-silver, platinum group metals, rare earths and so on.
- DY272 Nickel cobalt separation extractant, it can take cobalt out from nickel cobalt solution, then leave pure nickel.
- DY984N copper solvent extraction reagent.
- QL256-2 Nichel Cobalt Mangan Co extractant.
- DY316 Lithium extractant.
- DY319 extractant de co-extracție de nichel cobalt de înaltă eficiență pentru reciclarea bateriilor, can take out nickel and cobalt together from Lithium battery electrolyte.
- DY366 Scandium extractant.
- DY377 efficient nickel and diamond separation extractant.