DY973N Медный экстрагент is used for the copper selective recovery in the hydrometallurgical processing of copper ores. It is a high-performance hydroxyoxime compound solvent extraction (SX) reagent for copper ions. Specifically used for SX-EW circuits that treating high-content copper ores and low-pH heap leaching solutions.
This image shows the results of our copper extraction experiment, providing a clear understanding of its extraction principle:

This is the actual copper extraction plant, you can see the extracted pure copper sulfate:

Following are the instructions of DY973N:
1. Химический состав & Blending Ratio of DY973N:
Active Ingredients: 5-nonyl salicylaldoxime (Альдоксим) combined mixed with 2-hydroxy-5-nonyl acetophenone oxime (кетоксим).
Typical Active Ratio: Formulated in an optimized 7:3 volume ratio of aldoxime to ketoxime, includes 35% альдоксим, 15% кетоксим и 50% 260# растворяющее масло. The high aldoxime percentage delivers severe copper-loading payloads, while the paired ketoxime functions as a mild kinetic modifier.
2. Performance Parameters of DY973N:
| Physical form: | Technical Value |
| Появление | Fluid amber oil liquid |
| Плотность (25°С) | 0.91-0.93 |
| точка возгорания | ≥62°С (ПМКК) |
| Copper complex solubility (25°С) | ≥30 г/л Cu |
| Performance specifications: | |
| Maximum copper loading 10% (В/В) | 5.4-5.7 г/л меди |
| Изотермическая точка экстракции (Органический) | ≥4,7 г/л Cu |
| Кинетика экстракции | ≥95% (30s) |
| Extraction Cu/Fe selectivity | ≥2300 |
| Extraction phase separating | ≤70 с |
| Strip isotherm point | ≤2,0 г/л Cu |
| Net copper transfer | 2.7 г/л меди |
| Strip kinetics | ≥95% (30s) |
| Strip Phase separating | ≤80 с |
3. The Advantages of DY973N copper extractant:
Reduced Reagent Consumption: На практике, the consumption of single aldoxime will be 10 kg per metric ton cathode copper, but the consumption of DY973N will be under 5 kg per metric ton, will save the operating cost. Так, you can top up the active organic phase with DY973N copper extractant in any ratio.
Superior Iron Rejection: With a selectivity threshold surpassing 2,300, will effectively lock out ferric iron.
4. Application scopes of DY973N copper extractant:
High-Grade Copper Leaching: Used for circuits encountering highly concentrated base metal PLS.
Low-pH Heap & выщелачивание: Ideal for mineral acid levels in the pregnant leach solution (Пожалуйста) fluctuate significantly or sit at low baselines.
Recycle Scrap Processing: To recycle copper from industrial etching effluents.
Поэтому, if you want to verify the miscible compatibility of DY973N with your current active organic phase, пожалуйста свяжитесь с нами.
Кстати, наши экстрагенты металлов, как показано ниже, если тебе это нужно, пожалуйста, не стесняйтесь спрашивать нас:
- P204 (D2EHPA или HDEHP) Используется на первом этапе удаления примесей из латеритной никелевой руды..
- P507 экстрагент цветных металлов для меди, цинк, кобальт-никель, кадмий, золото серебро, металлы платиновой группы, редкоземельные элементы и так далее.
- DY272 Экстрагент для разделения никеля и кобальта, он может извлекать кобальт из раствора никеля-кобальта, тогда оставь чистый никель.
- DY984N реагент для экстракции меди растворителем.
- QL256-2 Никель Кобальт Марганец Совместная экстракция Экстрагент.
- DY316 Экстрагент лития.
- ДИ319 Высокоэффективный экстрагент для совместной экстракции никеля и кобальта для переработки аккумуляторов, может удалять никель и кобальт из электролита литиевой батареи.
- ДИ366 Экстрагент скандия.
- ДИ377 эффективный экстрагент для разделения никеля и алмазов.