Máy chiết đồng DY973N is used for the copper selective recovery in the hydrometallurgical processing of copper ores. It is a high-performance hydroxyoxime compound solvent extraction (SX) reagent for copper ions. Specifically used for SX-EW circuits that treating high-content copper ores and low-pH heap leaching solutions.
This image shows the results of our copper extraction experiment, providing a clear understanding of its extraction principle:

This is the actual copper extraction plant, you can see the extracted pure copper sulfate:

Following are the instructions of DY973N:
1. Chemical Composition & Blending Ratio of DY973N:
Active Ingredients: 5-nonyl salicylaldoxime (Aldoxime) combined mixed with 2-hydroxy-5-nonyl acetophenone oxime (Ketoxime).
Typical Active Ratio: Formulated in an optimized 7:3 volume ratio of aldoxime to ketoxime, includes 35% aldoxime, 15% xetonoxim và 50% 260# dầu dung môi. The high aldoxime percentage delivers severe copper-loading payloads, while the paired ketoxime functions as a mild kinetic modifier.
2. Performance Parameters of DY973N:
| Physical form: | Technical Value |
| Vẻ bề ngoài | Fluid amber oil liquid |
| Tỉ trọng (25°C) | 0.91-0.93 |
| Điểm sáng | ≥62 ° C (PMCC) |
| Copper complex solubility (25°C) | ≥30 g / L Cu |
| Performance specifications: | |
| Maximum copper loading 10% (V / V) | 5.4-5.7 g / L Cu |
| Khai thác điểm đẳng nhiệt (Hữu cơ) | ≥4,7 g/L Cu |
| Động học chiết xuất | ≥95% (30S) |
| Extraction Cu/Fe selectivity | ≥2300 |
| Extraction phase separating | ≤70 giây |
| Strip isotherm point | 2,0 g/L Cu |
| Net copper transfer | 2.7 g / L Cu |
| Strip kinetics | ≥95% (30S) |
| Strip Phase separating | ≤80 giây |
3. The Advantages of DY973N copper extractant:
Reduced Reagent Consumption: Trong thực tế, the consumption of single aldoxime will be 10 kg per metric ton cathode copper, but the consumption of DY973N will be under 5 kg per metric ton, will save the operating cost. So, you can top up the active organic phase with DY973N copper extractant in any ratio.
Superior Iron Rejection: With a selectivity threshold surpassing 2,300, will effectively lock out ferric iron.
4. Application scopes of DY973N copper extractant:
High-Grade Copper Leaching: Used for circuits encountering highly concentrated base metal PLS.
Low-pH Heap & Lọc: Ideal for mineral acid levels in the pregnant leach solution (XIN VUI LÒNG) fluctuate significantly or sit at low baselines.
Recycle Scrap Processing: To recycle copper from industrial etching effluents.
Do đó, if you want to verify the miscible compatibility of DY973N with your current active organic phase, xin vui lòng liên hệ với chúng tôi.
Nhân tiện, chất chiết kim loại của chúng tôi như dưới đây, nếu bạn cần nó, please feel free to ask us:
- P204 (D2EHPA hoặc HDEHP) Điều này được sử dụng cho bước đầu tiên để loại bỏ tạp chất cho quặng niken đá ong.
- P507 chất chiết kim loại màu cho đồng, kẽm, coban-niken, cadimi, vàng bạc, kim loại nhóm bạch kim, đất hiếm và như vậy.
- DY272 Chất chiết tách niken coban, nó có thể lấy coban ra khỏi dung dịch coban niken, sau đó để lại niken nguyên chất.
- DY984N thuốc thử chiết dung môi đồng.
- QL256-2 Chất chiết xuất đồng mangan Niken Cobalt.
- DY316 Lithium extractant.
- DY319 chất chiết đồng coban niken hiệu quả cao để tái chế pin, có thể loại bỏ niken và coban cùng nhau từ chất điện phân pin Lithium.
- DY366 Scandium extractant.
- DY377 efficient nickel and diamond separation extractant.